lnconel 617 is a nickel-chromium-cobalt-molybdenum alloy with an exceptional combination of metallurgical stability, strength, and oxidation resistance at high temperatures. Resistance to oxidation is enhanced by an aluminum addition. The alloy also resists a wide range of corrosive aqueous environments. Used in gas turbines for combustion cans, ducting, and transition liners; for petrochemical processing; for heat-treating equipment. Standard product forms are round, forging stock, extruded section, plate, sheet, strip, pipe, tube, and wire.
Nickel: 44.5 min
Chromium: 20.0-24.0
Cobalt: 10.0-15.0
Molybdenum: 8.0-10.0
Aluminum: 0.8-1.5
Carbon: 0.05-0.15
Iron: 3.0 max
Manganese: 1.0 max
Silicon:m1 .0 max
Sulfur: 0.015 max
Titanium: 0.6 max
Copper: 0.5 max
Boron: 0.006 max
Density: 0.302 lb/in3, 8.36 g/cm3
Electrical Resistivity: ohm-cir-mil/ft (micro-ohm-m):
At 78 ° F (20 ° C): 736 (1.222)
At 200 ° F (100 ° C): 448 (1.245)
At 400 ° F (200 ° C): 757 (1.258)
At 600 ° F (300 ° C): 764 (1.268)
At 800 ° F (400 ° C): 770 (1.278)
At 1000 ° F (500 ° C): 779 (1.290)
At 1200 ° F (600 ° C): 793 (1.308)
At 1400 ° F (700 ° C): 807 (1.332)
At 1600 ° F (800 ° C): 803 (1.342)
At 1800 ° F (900 ° C): 824 (1.338)
At 2000 ° F (1000 °C): - (1.378)
Specific Heat: BTU/lb-° F (J/Kg-° C):
At 78 ° F (20 ° C): 0.100 (419)
Thermal Conductivity: BTU-in/hr-tt2-° F (W/m•° C):
At 78 ° F (20 ° C): 94 ( 13.4) At 200 ° F (100 ° C): 101 (14.7)
At 400 ° F (200 ° C): 113 (16.3)
At 600 ° F (300 ° C): 125 (17.7)
At 800 ° F (400 ° C): 137 (19.3)
At 1000 ° F (500 ° C): 149 (20.9)
At 1200 ° F (600 ° C): 161 (22.5)
At 1400 ° F (700 ° C): 173 (23.9)
At 1600 ° F (800 ° C): 185 (25.5)
At 1800 ° F (900 ° C): 197 (27.1)
At 2000 ° F (1000 °C): 209 (28.7)
Mean Coefficient of Thermal Expansion: µin/in-° F(µm/m-° C):
78 - 200 ° F (20 - 100 ° C): 7.0 (11.6)
78 - 400 ° F (20 - 200 ° C): 7.2 (12.6)
78 - 600 ° F (20 - 300 ° C): 7.49 (13.1)
78 - 800 ° F (20 - 400 ° C): 7.6 (13.6)
78 - 1000 ° F (20 - 500 ° C: 7.7 (13.9)
78 - 1200 ° F (20 - 600 ° C): 8.0 (14.0)
78 - 1400 ° F (20 - 700 ° C): 8.4 (14.8)
78 - 1600 ° F (20 - 800 ° C): 8.7 (15.4)
78 - 1800 ° F (20 - 900 ° C): 9.0 (15.8)
78 - 2000 ° F (20 - 1000 °C): 9.2 (16.3)
Modulus of Elasticity: KSI (MPa):
30.6 x 103 (211 x 103) in tension
Melting Range: 2430 - 2510 ° F (1332 - 1380 ° C)
Coil - Sheet, Strip, Foil Wire - Profile, Round, Flat, Square
Ultimate Tensile Strength: 95 KSI min (655 MPa min)
Yield Strength: 35 KSI min (241 MPa min )
Elongation: 30% min
lnconel 617 can be cold worked to various tempers. Contact Ulbrich Technical Service for additional information.